Ok, I've seen quite a few responses to this posting & have been
wondering about some techniques I saw in the Dayton, OH weak signals
show I went to last year. While there, I saw a demo of mold use where
fiberglass cloth was applied to foam with a vaccuume system & a mold
where a sacrificial membrane was used against the mold in order to
provide a ready to show released part. The demonstrator even went so far
as to spray paint the sacrificial membraine prior to applying the
fiberglass & core material. When the part was extracted, not only did it
look good, BUT IT WAS ALREADY PAINTED!
Does anyone know if this is in use today for larger parts?