Thread: ice melt
View Single Post
  #2  
Old February 18th 05, 09:34 PM
Franklin Newton
external usenet poster
 
Posts: n/a
Default


"Blueskies" wrote in message
...

We started getting quite a few of our pups back from European operators

with the cad plated parts very corroded. Turns
out the Europeans were using some sort of new deicer stuff on their

runways and all. Unfortunately I do not know what
it was exactly, but you can do some testing on your own parts. Get some

old screw hardware from your local mechanic
and see what happens...


That pups should be pumps, as in hydraulic.
http://www.parker.com/ag/pdf/abexbrochure.pdf in case you are

interested...


Cadmium plating is routinely stripped from the base metal using an amonium
nitrate solution, hence the corrosion.