View Single Post
  #24  
Old March 15th 06, 07:12 PM posted to rec.aviation.homebuilt
external usenet poster
 
Posts: n/a
Default LCD Anodizing was More LED's - Again

"RST Engineering" wrote in news:3bb78$44185ad4
:

That would be great, if you would. However, he does seem to be quite
interested in selling his proprietary dye, desmutter, and sealant.

Jim



"John T" wrote in message
...
FWIW, I do have this guys instruction manual-if its the same guy
(adonizing aluminium). I can find the manual and look stuff up if you
want.




I came across this site a couple of years ago, when I thought I had time
to play It also tries to sell kits, but there are some manuals and
videos that made for some interesting reading. A lot of technical details
that convinced me that for the one or two pieces I wanted to do, I should
just have them done

http://support.caswellplating.com/

Jeff