#13
|
|||
|
|||
![]() Using lye ( sodium hydroxide ) for an etch is a disasterous choice. --------------------------------------------- Not necessarily. Not all aluminum is Alclad and sodium hydroxide has long been a standard for surface preparation for aluminum. But as with heat treatment or re-forming, it isn't an amateur sport :-) -R.S.Hoover |